Table 1. Certified Values for ZBK 306 (Mass Fraction %)
Number |
Elements |
TFe |
FeO |
SiO2 |
Al2O3 |
CaO |
MgO |
ZBK 306 |
Certified Values |
65.66 |
0.54 |
1.92 |
1.64 |
0.056 |
0.102 |
Uncertainty |
0.17 |
0.06 |
0.04 |
0.04 |
0.006 |
0.008 |
|
Number |
Elements |
S |
P |
Mn |
Ti |
K2O |
Na2O |
ZBK 306 |
Certified Values |
0.022 |
0.060 |
0.135 |
0.048 |
0.018 |
0.007 |
Uncertainty |
0.001 |
0.002 |
0.003 |
0.002 |
0.002 |
0.002 |
Table 2. Analysis methods
Composition |
Method |
TFe |
Titanium(III) chloride reduction potassium dichromate titration method |
FeO |
Potassium dichromate titration methodThe potentiometric titrimetric method |
SiO2 |
Perchloric acid dehydration gravimetric methodThe silicomolybdic blue spectrophotometric methodICP-AES |
Al2O3 |
Complexometric titration methodThe chrome azurol S photometric methodICP-AES |
CaO |
ICP-AESAAS |
MgO |
ICP-AESAAS |
S |
Barium sulfate gravimetric methodThe eombustion iodometric method for the determination of sulfur content |
P |
Bismuth phosphomolybdate blue spectrophotometric methodICP-AES |
Mn |
Potassium periodate spectrophotometric methodICP-AESAAS |
Ti |
Diantipyryl methane photometric methodICP-AES |
K2O |
ICP-AES AAS |
Na2O |
ICP-AES AAS |
Expiration of certification: The certification of this CRM is valid until December 1, 2028.
Table 3. Methods for homogeneity testing
Composition |
Analysis methods |
Minimum sample (g) |
TFe |
Titanium(III) chloride reduction potassium dichromate titration method |
0.2 |
FeO |
Potassium dichromate titration method |
0.2 |
SiO2, Al2O3, CaO, MgO |
ICP-AES |
0.1 |
Mn, Ti |
ICP-AES |
0.2 |
P, K2O, Na2O |
ICP-AES |
0.5 |
S |
The eombustion iodometric method for the determination of sulfur content |
0.5 |
The certified reference material is packed in glass bottles with plastic covers. The net weight is 70 g each. It is suggested to keep dryness when stored. The certified reference material should be dried at 105℃ for 1 hour before use, then it should be taken out and cooled to room temperature.
Product detail pictures:
Related Product Guide:
With our leading technology as well as our spirit of innovation,mutual cooperation, benefits and development, we will build a prosperous future together with your esteemed company for China Lignite Anthracite – Certified Reference Material – Shandong Institute of Metallurgical Science , The product will supply to all over the world, such as: El Salvador, Holland, Swiss, We pursue the management tenet of "Quality is superior, Service is supreme, Reputation is first", and will sincerely create and share success with all clients. We welcome you to contact us for more information and look forward to working with you.
By Pamela from Singapore - 2017.12.19 11:10
A good manufacturers, we have cooperated twice, good quality and good service attitude.
By Mabel from Italy - 2017.07.07 13:00