China Hsla Steel Manufacturer – Coke Series National And Industrial Reference Materials – Shandong Institute of Metallurgical Science
China Hsla Steel Manufacturer – Coke Series National And Industrial Reference Materials – Shandong Institute of Metallurgical Science Detail:
Table 1. Certified Values for GSB 03-2022-2006 (Mass Fraction %)
Number |
Elements |
TFe |
FeO |
SiO2 |
Al2O3 |
CaO |
MgO |
S |
GSB 03-2022-2006 |
Certified Values |
61.53 |
0.24 |
3.43 |
2.12 |
0.118 |
0.109 |
0.038 |
Uncertainty |
0.10 |
0.01 |
0.04 |
0.05 |
0.007 |
0.005 |
0.002 |
|
Number |
Elements |
P |
Mn |
Ti |
K2O |
Na2O |
Cu |
Ni |
GSB 03-2022-2006 |
Certified Values |
0.068 |
0.276 |
0.052 |
0.026 |
0.034 |
0.0014 |
0.0027 |
Uncertainty |
0.002 |
0.005 |
0.002 |
0.003 |
0.003 |
0.0002 |
0.0003. |
|
Number |
Elements |
Co |
As |
Pb |
Zn |
Cr |
|
|
GSB 03-2022-2006 |
Certified Values |
0.0009 |
0.0011 |
0.0008 |
0.0020 |
0.0054 |
|
|
Uncertainty |
0.0001 |
0.0002 |
0.0001 |
0.0003 |
0.0004 |
|
Table 2. Analysis Methods
Composition |
Method |
TFe |
Titrimetric method after tin (Ⅱ) chloride reduction Titanium (Ⅲ) chloride reduce potassium dichromate titration method |
FeO |
Potassium dichromate titration method Sulfosalicylic acid spectrophotometric method Potentiometric titration method |
SiO2 |
Perchloric acid dehydration gravimetric method The silicomolybdic blue spectrophotometric method ICP-AES |
CaO |
AAS ICP-AES |
MgO |
AAS ICP-AES |
Al2O3 |
EDTA titrimetric method ICP-AES |
Ti |
ICP-AES Diantipyrylmethane spectrophotometric method |
Mn |
ICP-AES AAS Potassium periodate spectrophotometric method |
P |
N-butyl alcohol-chloroform extraction molybdenum blue spectrophotome-tric method The butyl acetate extraction photometric method Phosphovanoclonoiybeate molecular absorption spectromrtric method Bismuth phosphomolybdenum blue photometry ICP-AES |
S |
High frequency combustion infrared absorption method Barium sulfate gravimetric method Combustion iodometric method |
K2O |
ICP-AES AAS |
Na2O |
ICP-AES AAS |
Cu |
ICP-AES AAS GFAAS |
Ni |
AAS GFAAS ICP-AES |
Co |
AAS GFAAS ICP-AES |
As |
Silver diethyldithiocarbamate spectrophotometry Arseno molybdenum blue spectrophotometric method after the extraction separation GFAAS HGAAS ICP-AES |
Pb |
GFAAS AAS ICP-AES ICP-MS |
Zn |
ICP-AES AAS |
Cr |
AAS GFAAS ICP-AES |
The certified reference material is packed in glass bottles with plastic covers. The net weight is 50g each. It is suggested to keep dryness when stored. The certified reference material should be dried at 105℃ for 1 hour before use, then it should be taken out and cooled to room temperature.
Product detail pictures:
Related Product Guide:
abide by the contract", conforms on the market requirement, joins within the market competition by its superior quality likewise as provides far more comprehensive and great company for shoppers to let them develop into huge winner. The pursue on the corporation, is definitely the clients' gratification for China Hsla Steel Manufacturer – Coke Series National And Industrial Reference Materials – Shandong Institute of Metallurgical Science , The product will supply to all over the world, such as: Australia, Guinea, Toronto, Based on our automatic production line, steady material purchase channel and quick subcontract systems have been built in mainland China to meet customer's wider and higher requirement in recent years. We have been looking forward to cooperating with more clients worldwide for common development and mutual benefit!Your trust and approval are the best reward for our efforts. Keeping honest, innovative and efficient, we sincerely expect that we can be business partners to create our brilliant future!
By Kevin Ellyson from Armenia - 2018.02.12 14:52
The company has a good reputation in this industry, and finally it tured out that choose them is a good choice.
By Ellen from Venezuela - 2017.06.25 12:48