Certified Reference Material

products

Certified Reference Material

Short Description:

The CRM is used for the quality control and calibration of analytical instruments in analysis of Iron Ore. It is also used for the evaluation and verification of accuracy of the analytical methods. The CRM can be used for the transfer of measured value.


Product Detail

Product Tags

Product introduction

Chemical Analysis (1)
Chemical Analysis (2)

Certified Values

Table 1. Certified Values for ZBK 306 (Mass Fraction %)

Number

Elements

TFe

FeO

SiO2

Al2O3

CaO

MgO

ZBK 306

Certified Values

65.66

0.54

1.92

1.64

0.056

0.102

Uncertainty

0.17

0.06

0.04

0.04

0.006

0.008

Number

Elements

S

P

Mn

Ti

K2O

Na2O

ZBK 306

Certified Values

0.022

0.060

0.135

0.048

0.018

0.007

Uncertainty

0.001

0.002

0.003

0.002

0.002

0.002

Analysis Methods

Table 2. Analysis methods

Composition

Method

TFe

Titanium(III) chloride reduction potassium dichromate titration method

FeO

Potassium dichromate titration methodThe potentiometric titrimetric method

SiO2

Perchloric acid dehydration gravimetric methodThe silicomolybdic blue spectrophotometric methodICP-AES

Al2O3

Complexometric titration methodThe chrome azurol S photometric methodICP-AES

CaO

ICP-AESAAS

MgO

ICP-AESAAS

S

Barium sulfate gravimetric methodThe eombustion iodometric method for the determination of sulfur content

P

Bismuth phosphomolybdate blue spectrophotometric methodICP-AES

Mn

Potassium periodate spectrophotometric methodICP-AESAAS

Ti

Diantipyryl methane photometric methodICP-AES

K2O

ICP-AES AAS

Na2O

ICP-AES AAS

Homogeneity Test and Stability Inspection

Expiration of certification: The certification of this CRM is valid until December 1, 2028.

Table 3. Methods for homogeneity testing

Composition

Analysis methods

Minimum sample (g)

TFe

Titanium(III) chloride reduction potassium dichromate titration method

0.2

FeO

Potassium dichromate titration method

0.2

SiO2, Al2O3, CaO, MgO

ICP-AES

0.1

Mn, Ti

ICP-AES

0.2

P, K2O, Na2O

ICP-AES

0.5

S

The eombustion iodometric method for the determination of sulfur content

0.5

Packing and Storage

The certified reference material is packed in glass bottles with plastic covers. The net weight is 70 g each. It is suggested to keep dryness when stored. The certified reference material should be dried at 105℃ for 1 hour before use, then it should be taken out and cooled to room temperature.


  • Previous:
  • Next:

  • Write your message here and send it to us