Table 1. Certified Values for ZBK 306 (Mass Fraction %)
Number |
Elements |
TFe |
FeO |
SiO2 |
Al2O3 |
CaO |
MgO |
ZBK 306 |
Certified Values |
65.66 |
0.54 |
1.92 |
1.64 |
0.056 |
0.102 |
Uncertainty |
0.17 |
0.06 |
0.04 |
0.04 |
0.006 |
0.008 |
|
Number |
Elements |
S |
P |
Mn |
Ti |
K2O |
Na2O |
ZBK 306 |
Certified Values |
0.022 |
0.060 |
0.135 |
0.048 |
0.018 |
0.007 |
Uncertainty |
0.001 |
0.002 |
0.003 |
0.002 |
0.002 |
0.002 |
Table 2. Analysis methods
Composition |
Method |
TFe |
Titanium(III) chloride reduction potassium dichromate titration method |
FeO |
Potassium dichromate titration methodThe potentiometric titrimetric method |
SiO2 |
Perchloric acid dehydration gravimetric methodThe silicomolybdic blue spectrophotometric methodICP-AES |
Al2O3 |
Complexometric titration methodThe chrome azurol S photometric methodICP-AES |
CaO |
ICP-AESAAS |
MgO |
ICP-AESAAS |
S |
Barium sulfate gravimetric methodThe eombustion iodometric method for the determination of sulfur content |
P |
Bismuth phosphomolybdate blue spectrophotometric methodICP-AES |
Mn |
Potassium periodate spectrophotometric methodICP-AESAAS |
Ti |
Diantipyryl methane photometric methodICP-AES |
K2O |
ICP-AES AAS |
Na2O |
ICP-AES AAS |
Expiration of certification: The certification of this CRM is valid until December 1, 2028.
Table 3. Methods for homogeneity testing
Composition |
Analysis methods |
Minimum sample (g) |
TFe |
Titanium(III) chloride reduction potassium dichromate titration method |
0.2 |
FeO |
Potassium dichromate titration method |
0.2 |
SiO2, Al2O3, CaO, MgO |
ICP-AES |
0.1 |
Mn, Ti |
ICP-AES |
0.2 |
P, K2O, Na2O |
ICP-AES |
0.5 |
S |
The eombustion iodometric method for the determination of sulfur content |
0.5 |
The certified reference material is packed in glass bottles with plastic covers. The net weight is 70 g each. It is suggested to keep dryness when stored. The certified reference material should be dried at 105℃ for 1 hour before use, then it should be taken out and cooled to room temperature.
Product detail pictures:
Related Product Guide:
We've been convinced that with joint efforts, the enterprise between us will bring us mutual benefits. We are able to assure you product or service quality and aggressive cost for Bituminous Coal For Blacksmithing Supplier – Certified Reference Material – Shandong Institute of Metallurgical Science , The product will supply to all over the world, such as: azerbaijan, Serbia, Israel, With a fully integrated operation system, our company has won a good fame for our high quality goods, reasonable prices and good services. Meanwhile, we have established a strict quality management system conducted in material incoming, processing and delivery. Abiding by the principle of "Credit first and customer supremacy", we sincerely welcome clients from home and abroad to cooperate with us and advance together to create a brilliant future.
By Renee from Colombia - 2017.07.07 13:00
We are really happy to find such a manufacturer that ensuring product quality at the same time the price is very cheap.
By ROGER Rivkin from Uruguay - 2018.11.28 16:25