17034 Iso Factory – Certified Reference Material – Shandong Institute of Metallurgical Science
17034 Iso Factory – Certified Reference Material – Shandong Institute of Metallurgical Science Detail:
Table 1. Certified Values for ZBK 306 (Mass Fraction %)
Number |
Elements |
TFe |
FeO |
SiO2 |
Al2O3 |
CaO |
MgO |
ZBK 306 |
Certified Values |
65.66 |
0.54 |
1.92 |
1.64 |
0.056 |
0.102 |
Uncertainty |
0.17 |
0.06 |
0.04 |
0.04 |
0.006 |
0.008 |
|
Number |
Elements |
S |
P |
Mn |
Ti |
K2O |
Na2O |
ZBK 306 |
Certified Values |
0.022 |
0.060 |
0.135 |
0.048 |
0.018 |
0.007 |
Uncertainty |
0.001 |
0.002 |
0.003 |
0.002 |
0.002 |
0.002 |
Table 2. Analysis methods
Composition |
Method |
TFe |
Titanium(III) chloride reduction potassium dichromate titration method |
FeO |
Potassium dichromate titration methodThe potentiometric titrimetric method |
SiO2 |
Perchloric acid dehydration gravimetric methodThe silicomolybdic blue spectrophotometric methodICP-AES |
Al2O3 |
Complexometric titration methodThe chrome azurol S photometric methodICP-AES |
CaO |
ICP-AESAAS |
MgO |
ICP-AESAAS |
S |
Barium sulfate gravimetric methodThe eombustion iodometric method for the determination of sulfur content |
P |
Bismuth phosphomolybdate blue spectrophotometric methodICP-AES |
Mn |
Potassium periodate spectrophotometric methodICP-AESAAS |
Ti |
Diantipyryl methane photometric methodICP-AES |
K2O |
ICP-AES AAS |
Na2O |
ICP-AES AAS |
Expiration of certification: The certification of this CRM is valid until December 1, 2028.
Table 3. Methods for homogeneity testing
Composition |
Analysis methods |
Minimum sample (g) |
TFe |
Titanium(III) chloride reduction potassium dichromate titration method |
0.2 |
FeO |
Potassium dichromate titration method |
0.2 |
SiO2, Al2O3, CaO, MgO |
ICP-AES |
0.1 |
Mn, Ti |
ICP-AES |
0.2 |
P, K2O, Na2O |
ICP-AES |
0.5 |
S |
The eombustion iodometric method for the determination of sulfur content |
0.5 |
The certified reference material is packed in glass bottles with plastic covers. The net weight is 70 g each. It is suggested to keep dryness when stored. The certified reference material should be dried at 105℃ for 1 hour before use, then it should be taken out and cooled to room temperature.
Product detail pictures:
Related Product Guide:
We also offer product sourcing and flight consolidation services. We've got our personal factory and sourcing office. We can easily present you with almost every style of merchandise linked to our merchandise range for 17034 Iso Factory – Certified Reference Material – Shandong Institute of Metallurgical Science , The product will supply to all over the world, such as: Oman, Pakistan, Romania, Our company will continue to serve customers with best quality, competitive price and timely delivery & the best payment term! We sincerely welcome friends from all over the world to visit& cooperate with us and enlarge our business. If you are interested in our products, please do not hesitate to contact us, we will be happy to provide you with further information!
By Fernando from Washington - 2017.07.28 15:46
Good quality and fast delivery, it's very nice. Some products have a little bit problem, but the supplier replaced timely, overall, we are satisfied.
By Kama from Mali - 2018.06.03 10:17